Ytterbium Doped Yttrium Aluminum Garnet
Yb:YAG crystal is one of the most promising laser-active materials and more suitable for diode-pumping than the traditional nd-doped systems. It can be pumped at 0.94mm laser output. Compared with the commonly used Nd:YAG crystal, Yb:YAG crystal has a much larger absorption bandwidth to reduces thermal management requirements for diode lasers, a longer upper-state lifetime, three to four times lower thermal loading per unit pump power. Yb:YAG crystal is expected to replace Nd:YAG crystal for high power diode-pumped lasers and other potential applications.
We has recently developed a suitable technique to produce the Yb:YAG crystal High quality Yb:YAG crystals are available with different specifications.
Main Advantages:
Very low fractional heating, less than < 11%
Very high slope efficiency
Broad absorption bands, about 18nm @ 940nm
No excited-state absorption or up-conversion
Conveniently pumped by reliable InGaAs diodes at 940nm (or 970nm)
High thermal conductivity and strength
Basic properties:
Chemical Formula
|
Yb:Y3Al5O12
|
Crystal Structure
|
Cubic
|
Lattice Constants
|
12.01
|
Melting Point
|
1970 ℃
|
Density
|
4.56 g/cm2
|
Mohs Hardness
|
8.5
|
Dopant
|
5~30% Yb
|
Thermal Expansion Coefficient
|
7.8´10-6 /K, [111], 0-250℃
|
Thermal Conductivity
|
14 W×s /m /K @ 20℃
|
Loss Coefficient
|
0.003 cm-1
|
Index of Refraction
|
1.82
|
dn/dT
|
9´10-6/℃
|
Lasing Wavelength
|
1030nm, 1050nm
|
Fluorescence lifetime
|
1.2ms
|
Emission cross section
|
2.2´10-20cm2
|
Pump Wavelength
|
0.9~1.0mm
|
Absorption band about pump wavelength
|
18nm
|
Main Specification:
Diameter Tolerance
|
+0.0,-0.1mm, ±0.05mm
|
Thickness Tolerance
|
±0.02mm(standard), ±0.01mm(special)
|
Three-dimensional Tolerance
|
±0.02x±0.03±0.02mm
|
Parallelism
|
<30’
|
Flatness
|
λ/8
|
Perpendicularity
|
<10”
|
Scratch-Dig
|
5-10 per MIL-O-13830a
|
Wavefront Distortion
|
<λ/2 per inch(λ@1064nm)
|